Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

LyondellBasell Alathon® H4250 High Density Polyethylene, Injection Molding Grade

Category Polymer , Thermoplastic , Polyethylene (PE) , HDPE , High Density Polyethylene (HDPE), Injection Molded
Manufacturer LyondellBasell (former Equistar)
Trade Name Alathon®
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF LyondellBasell Alathon® H4250 High Density Polyethylene, Injection Molding Grade.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
ALATHON H4250 is a high-flow “freezer” grade resin that exhibits enhanced cold temperature impact performance, enhanced processing and thermal stability, with good color and organoleptic properties. Typical applications are rigid food containers such as four, five and six-quart ice cream containers that are produced at high speeds in fast cycling multi-cavity stack molds. Regulatory Status: H4250 meets the requirements of the Food and Drug Administration regulation 21 CFR 177.1520. This regulation allows the use of this olefin polymer in "...articles or components of articles intended for use in contact with food." Specific limitations or conditions of use may apply. Contact your Equistar sales representative for more information. Specific recommendations for processing H4250 can only be made when the processing conditions, equipment and end use application are knownThis product is from the former Equistar product line.
Physical Properties Metric English Comments
Bulk Density 0.593 - 0.625 g/cc
0.0214 - 0.0226 lb/in³
ASTM D1895
Density 0.942 g/cc
0.0340 lb/in³
ASTM D1505
Melt Flow 50 g/10 min

@Load 2.16 kg,
Temperature 190 °C
50 g/10 min

@Load 4.76 lb,
Temperature 374 °F
ASTM D1238
Spiral Flow 43.7 cm
17.2 in
Equistar test
Mechanical Properties Metric English Comments
Hardness, Shore D 61
61
ASTM D2240
Tensile Strength at Break 21.1 MPa
3060 psi
50 mm/min; ASTM D638
Elongation at Break 12 %
12 %
50 mm/min; ASTM D638
Tensile Modulus 0.6922 GPa
100.4 ksi
1% Secant; 50mm/min; ASTM D638
0.9425 GPa
136.7 ksi
50mm/min; ASTM D638
Flexural Modulus 0.7040 GPa
102.1 ksi
2% Secant; 12.5 mm/min; ASTM D790
0.8260 GPa
119.8 ksi
1% Secant; 12.5 mm/min; ASTM D790
0.9411 GPa
136.5 ksi
12.5 mm/min; ASTM D790
Izod Impact, Notched 0.347 J/cm
0.650 ft-lb/in
ASTM D256
NB

@Temperature -18.0 °C
NB

@Temperature -0.400 °F
ASTM D4812
Thermal Properties Metric English Comments
Melting Point 124.0 °C
255.2 °F
ASTM D3418
Crystallization Temperature 112.5 °C
234.5 °F
ASTM D3418
Deflection Temperature at 0.46 MPa (66 psi) 59.5 °C
139 °F
ASTM D648
Vicat Softening Point 116 °C
241 °F
ASTM D1525
Processing Properties Metric English Comments
Rear Barrel Temperature 232 °C
450 °F
Middle Barrel Temperature 243 °C
470 °F
Front Barrel Temperature 246 °C
475 °F
Nozzle Temperature 246 °C
475 °F