LyondellBasell Alathon® H5220 High Density Polyethylene, Injection Molding Grade

Category Polymer , Thermoplastic , Polyethylene (PE) , HDPE , High Density Polyethylene (HDPE), Injection Molded
Manufacturer LyondellBasell (former Equistar)
Trade Name Alathon®
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF LyondellBasell Alathon® H5220 High Density Polyethylene, Injection Molding Grade.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
ApplicationsAlathon H5220 provides easy processing characteristics and exhibits excellent toughness properties and color as well as low odor and good processing stability. Typical applications include housewares, containers, caps and closures.Regulatory StatusH5220 meets the requirements of the Food and Drug Administration regulation 21 CFR 177.1520.Processing TechniquesSpecific recommendations for processing H5220 can only be made when the processing conditions, equipment and end-use applications are known.
Physical Properties Metric English Comments
Bulk Density 0.529 - 0.593 g/cc
0.0191 - 0.0214 lb/in³
ASTM D1895
Density 0.952 g/cc
0.0344 lb/in³
ASTM D1505
Melt Flow 20 g/10 min

@Load 0.980 kg,
Temperature 190 °C
20 g/10 min

@Load 2.16 lb,
Temperature 374 °F
ASTM D1238
Spiral Flow 29.5 cm
11.6 in
Equistar
Mechanical Properties Metric English Comments
Hardness, Shore D 76
76
ASTM D2240
Tensile Strength, Yield 26.1 MPa
3790 psi
50 mm/min, Type IV; ASTM D4796
Elongation at Yield 11 %
11 %
50 mm/min, Type IV; ASTM D638
Tensile Modulus 1.00 GPa
145 ksi
1% Secant, 50mm/min; ASTM D638
1.26 GPa
183 ksi
50 mm/min; ASTM D638
Flexural Modulus 1.25 GPa
181 ksi
ASTM D790
1% Secant Modulus 1080 MPa
157000 psi
12.5mm/min; ASTM D790
2% Secant Modulus 0.903 GPa
131 ksi
12.5mm/min; ASTM D790
Izod Impact, Notched 0.379 J/cm

@Temperature 23.0 °C
0.710 ft-lb/in

@Temperature 73.4 °F
ASTM D256
Izod Impact, Unnotched NB

@Temperature -18.0 °C
NB

@Temperature -0.400 °F
ASTM D4812
Thermal Properties Metric English Comments
Melting Point 130.2 °C
266.4 °F
ASTM D3418
Crystallization Temperature 115.4 °C
239.7 °F
ASTM D3418
Deflection Temperature at 0.46 MPa (66 psi) 72.8 °C
163 °F
ASTM D648
Vicat Softening Point 124 °C
256 °F
ASTM D1525
Brittleness Temperature <= -76.1 °C
<= -105 °F
F<sub>50</sub>; ASTM D746
Compliance Properties Metric English Comments
FDA Yes
Yes
Processing Properties Metric English Comments
Rear Barrel Temperature 232 °C
450 °F
Middle Barrel Temperature 243 °C
470 °F
Front Barrel Temperature 246 °C
475 °F
Nozzle Temperature 246 °C
475 °F
Copyright © lookpolymers.com All Rights Reserved