Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

LyondellBasell Alathon® L5008 High Density Polyethylene

Category Polymer , Thermoplastic , Polyethylene (PE) , HDPE , High Density Polyethylene (HDPE), Pipe Grade
Manufacturer LyondellBasell (former Equistar)
Trade Name Alathon®
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF LyondellBasell Alathon® L5008 High Density Polyethylene.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
ApplicationsALATHON L 5008 is a high molecular weight high density polyethylene copolymer resin with broad and bimodal molecular weight distribution.Regulatory StatusWhen L 5008 is compounded with an Equistar approved black concentrate it meets the following standards and classifications:Plastics Pipe Institute (PPI) PE3408 Standard Grade for pipe applications at 1600 psi HDB at 73°F (23°C).Plastics Pipe Institute (PPI) PE4608 (E4) Grade for pipe applications at 1000 psi HDB at 140°F (60°C).NSF Standard 14 and Standard 61 for Potable Water Pipe and Fittings.ASTM D 3350 Cell Classification 445564C.ProcessingSpecific recommendations for processing conditions can be made only when the equipment, conditions, and end use are known.This product is from the former Equistar product line.
Physical Properties Metric English Comments
Density 0.949 g/cc
0.0343 lb/in³
ASTM D1505
Melt Flow 0.070 g/10 min
0.070 g/10 min
ASTM D1238
High Load Melt Index 16 g/10 min
16 g/10 min
ASTM D1238
Mechanical Properties Metric English Comments
Tensile Strength at Break 35.2 MPa
5100 psi
ASTM D638
Tensile Strength, Yield 23.4 MPa
3400 psi
ASTM D638
Elongation at Break 800 %
800 %
ASTM D638
1% Secant Modulus 1100 MPa
160000 psi
ASTM D790
Thermal Properties Metric English Comments
Deflection Temperature at 0.46 MPa (66 psi) 76.0 °C
169 °F
ASTM D648
DSC Induction Temperature >= 250 °C
>= 482 °F
ASTM D3350
Copyright © lookpolymers.com All Rights Reserved