LyondellBasell Alathon® L5885 High Density Polyethylene

Category Polymer , Film , Thermoplastic , Polyethylene (PE) , HDPE , High Density Polyethylene (HDPE), Film Grade
Manufacturer LyondellBasell (former Equistar)
Trade Name Alathon®
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF LyondellBasell Alathon® L5885 High Density Polyethylene.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
ApplicationsALATHON L 5885 is a medium molecular weight high density homopolymer for use in blown film applications. Typical applications include those low WVTR requirements.Regulatory StatusL 5855 meets the requirements of Food and Drug Administration regulation, 21 CFR 177.1520. This regulation allows the use of this olefin polymer in "…articles or components of articles intended for use in contact with food." Specific limitations or conditions of use may apply. Contact your Equistar sales representative for more information. Processing TechniquesSpecific recommendations for processing LB 0100-00 can only be made when the processing conditions, equipment and end use are known. For further suggestions, please contact your Equistar sales representative.Typical Extrusion Conditions: 2.0 Mil Film; Melt Temperature- 390°-410°F(199°This product is from the former Equistar product line.
Physical Properties Metric English Comments
Density 0.958 g/cc
0.0346 lb/in³
ASTM D792
Thickness 50.8 microns
2.00 mil
Melt Flow 0.85 g/10 min
0.85 g/10 min
ASTM D1238
Mechanical Properties Metric English Comments
Film Tensile Strength at Yield, MD 25.5 MPa
3700 psi
ASTM D882
Film Tensile Strength at Yield, TD 26.2 MPa
3800 psi
ASTM D882
Film Elongation at Break, MD 700 %
700 %
ASTM D882
Film Elongation at Break, TD 750 %
750 %
ASTM D882
Elmendorf Tear Strength MD 18 g
18 g
ASTM D1922
Elmendorf Tear Strength TD 900 g
900 g
ASTM D1922
1% Secant Modulus, MD 862 MPa
125000 psi
ASTM D882
1% Secant Modulus, TD 1000 MPa
145000 psi
ASTM D822
Processing Properties Metric English Comments
Melt Temperature 199 - 210 °C
390 - 410 °F
Typical Extrusion