LyondellBasell Astryn BA36GC Polypropylene Copolymer

Category Polymer , Thermoplastic , Polypropylene (PP)
Manufacturer LyondellBasell
Trade Name Astryn
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF LyondellBasell Astryn BA36GC Polypropylene Copolymer.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Key Features: conventional melt flow, medium modulus, UV-stabilized polypropylene copolymer, moderate stiffness, good impact resistance, low foggingApplications: seat valances, passenger assist handles, coat hooksDescription: Astryn BA36GC conventional melt flow, UV-stabilized, precolored polypropylene copolymer has intermediate stiffness and good impact resistance. It was designed for a variety of automotive interior applications.Information provided by Montell Polyolefins.LyondellBasell is the successor company to Montell.
Physical Properties Metric English Comments
Density 0.900 g/cc
0.0325 lb/in³
ASTM D792B
Linear Mold Shrinkage 0.015 cm/cm
0.015 in/in
Tool, Montell
Melt Flow 6.0 g/10 min

@Load 2.16 kg,
Temperature 230 °C
6.0 g/10 min

@Load 4.76 lb,
Temperature 446 °F
ASTM D1238
Mechanical Properties Metric English Comments
Hardness, Shore D 61
61
ISO Method 868
Tensile Strength, Yield 26.0 MPa
3770 psi
ISO Method R527
Elongation at Yield 8.0 %
8.0 %
ASTM D638
Flexural Modulus 1.20 GPa
174 ksi
ISO Method 178
Izod Impact Resistance 0.740 J/cm²
3.52 ft-lb/in²
ISO 180
Thermal Properties Metric English Comments
CTE, linear 70.0 µm/m-°C

@Temperature -30.0 - 30.0 °C
38.9 µin/in-°F

@Temperature -22.0 - 86.0 °F
ASTM D696
Deflection Temperature at 0.46 MPa (66 psi) 93.0 °C
199 °F
ISO Method 75