Material Notes:
Description: DEXFLEX® 711 is a thermoplastic olefinic elastomer compounded with post-industrial/post-consumer recycled materials. It is designed for use in applications that are (non-color matched) black, and that require very good processing characteristics. Applications: Wheel liners, filler panels, fan shrouds, air dams, and sight shields Information provided by Solvay Engineered Polymers.LyondellBasell acquired Solvay Engineered Polymers in 2008.
Physical Properties Metric English Comments
Specific Gravity 0.940 g/cc
0.940 g/cc
ASTM D792
Linear Mold Shrinkage 0.010 cm/cm
0.010 in/in
ASTM D995
Melt Flow 11 g/10 min
11 g/10 min
ASTM D1238
Mechanical Properties Metric English Comments
Tensile Strength, Yield 19.0 MPa
2760 psi
50 mm/min, Type 4; ASTM D638
Flexural Modulus 0.860 GPa
125 ksi
0.05 in/min, 1x3"; ASTM D790
Thermal Properties Metric English Comments
CTE, linear 88.0 µm/m-°C

@Temperature 20.0 °C
48.9 µin/in-°F

@Temperature 68.0 °F
modified; ASTM D696