Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

LyondellBasell Hifaxâ„¢ CA10GC Thermoplastic Polyolefin Elastomer

Category Polymer , Thermoplastic , Elastomer, TPE , Thermoplastic Olefinic Elastomer (TPO) , Polyolefin
Manufacturer LyondellBasell
Trade Name Hifax™
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF LyondellBasell Hifaxâ„¢ CA10GC Thermoplastic Polyolefin Elastomer.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Description: Hifaxâ„¢ CA10GC fractional melt flow, 100 MPa flexural modulus, precolored, UV-stabilized, reactor grade, extrudable thermoplastic elastomeric olefin (TEO) resin combines good processability with balanced strength, toughness, flexibility and weatherability. It is based on material produced from proprietary Basell process technology and was designed primarily for applications requiring extended outdoor exposure. Uses: Sheet, geo membranesInformation provided by Basell.
Physical Properties Metric English Comments
Density 0.892 g/cc
0.0322 lb/in³
ASTM D792
Melt Flow 0.80 g/10 min

@Load 2.16 kg,
Temperature 230 °C
0.80 g/10 min

@Load 4.76 lb,
Temperature 446 °F
Condition L; ASTM D1238
Mechanical Properties Metric English Comments
Hardness, Shore D 43
43
ASTM D2240
Tensile Strength at Break 14.0 MPa
2030 psi
ASTM D 638
Tensile Strength, Yield 9.03 MPa
1310 psi
ASTM D 638
Elongation at Break 600 %
600 %
ASTM D 638
Flexural Modulus 0.0903 GPa
13.1 ksi
Tangent, 0.05 in/min; ASTM D790
0.100 GPa
14.5 ksi
Tangent, 0.5 in/min; ASTM D790
Tear Strength 78.9 kN/m
450 pli
ASTM D624
Users viewing this material also viewed the following: