Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

LyondellBasell Hifax™ CA207A Thermoplastic Polyolefin Elastomer

Category Polymer , Thermoplastic , Elastomer, TPE , Thermoplastic Olefinic Elastomer (TPO) , Polyolefin
Manufacturer LyondellBasell
Trade Name Hifax™
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF LyondellBasell Hifax™ CA207A Thermoplastic Polyolefin Elastomer.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Description: Hifax™ CA207A thermoplastic olefin resin is designed to reduce shrinkage and improve paint adhesion of PP compound. It is based on proprietary Basell process technology. All ingredients in "Hifax" CA207A resin meet the chemical registration requirements of TSCA (U.S.) and DSL (Canada). Uses: CompoundingInformation provided by Basell.
Physical Properties Metric English Comments
Density 0.892 g/cc
0.0322 lb/in³
ASTM D792
Melt Flow 8.0 g/10 min

@Load 2.16 kg,
Temperature 230 °C
8.0 g/10 min

@Load 4.76 lb,
Temperature 446 °F
Condition L; ASTM D1238
Mechanical Properties Metric English Comments
Hardness, Shore D 57
57
ASTM D2240
Tensile Strength, Yield 14.5 MPa
2100 psi
ASTM D 638
Elongation at Yield 23 %
23 %
ASTM D 638
Flexural Modulus 0.469 GPa
68.0 ksi
1% Secant, 0.05 in/min; ASTM D790
Izod Impact, Notched NB
NB
73°F; ASTM D256
Users viewing this material also viewed the following:
Copyright © lookpolymers.com All Rights Reserved