Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

LyondellBasell Hifax™ CB235 Thermoplastic Olefin Resin

Category Polymer , Thermoplastic
Manufacturer LyondellBasell
Trade Name Hifax™
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF LyondellBasell Hifax™ CB235 Thermoplastic Olefin Resin.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Key Features: medium high melt flow, medium high modulus, paintable thermoplastic olefin resin, excellent impact and stiffness balance, good dimensional stability, excellent processability, good paintabilityApplications: automotive claddings and rocker panels, appliques, filler panelsDescription: Hifax CB235 medium melt flow, paintable, mineral-filled thermoplastic olefin resin has an excellent combnation of impact rigidity and processability. It was designed primarily for automotive exterior ornamentation applications.Information provided by Montell Polyolefins.LyondellBasell is the successor company to Montell.
Physical Properties Metric English Comments
Density 0.930 g/cc
0.0336 lb/in³
ASTM D792
Linear Mold Shrinkage 0.010 cm/cm
0.010 in/in
Tool, Montell
Melt Flow 12 g/10 min

@Load 2.16 kg,
Temperature 230 °C
12 g/10 min

@Load 4.76 lb,
Temperature 446 °F
ASTM D1238
Mechanical Properties Metric English Comments
Hardness, Shore D 67
67
ASTM D2240
Tensile Strength, Yield 19.0 MPa
2760 psi
ASTM D638
Elongation at Break 400 %
400 %
ASTM D638
Elongation at Yield 12 %
12 %
ASTM D638
Flexural Modulus 0.960 GPa
139 ksi
Tangent at 0.05 in/min; ASTM D790A
Gardner Impact 28.0 J

@Temperature -30.0 °C
20.7 ft-lb

@Temperature -22.0 °F
ASTM D3029
Impact Test 23.0 J

@Temperature -30.0 °C
17.0 ft-lb

@Temperature -22.0 °F
Dynatup Impact, E at Max Load, Ductile; ASTM D3763
Tear Strength 110 kN/m
628 pli
ASTM D624