LyondellBasell Hifaxâ„¢ EP2015/60 Thermoplastic Polyolefin Elastomer

Category Polymer , Thermoplastic , Polypropylene (PP) , Polypropylene, Extrusion Grade
Manufacturer LyondellBasell
Trade Name Hifax™
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF LyondellBasell Hifaxâ„¢ EP2015/60 Thermoplastic Polyolefin Elastomer.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Description: Hifaxâ„¢ EP2015/60 medium melt flow, 690 MPa flexural modulus, extrusion coating grade, specialty polypropylene copolymer has a very good balance of properties and processability. This material was designed for use as an adhesive tie layer in various extrusion coating applications. Uses: Piping, coating applicationsInformation provided by Basell.
Physical Properties Metric English Comments
Density 0.892 g/cc
0.0322 lb/in³
ASTM D792
Melt Flow 10 g/10 min

@Load 2.16 kg,
Temperature 230 °C
10 g/10 min

@Load 4.76 lb,
Temperature 446 °F
Condition L; ASTM D1238
Mechanical Properties Metric English Comments
Hardness, Rockwell R 67
67
ASTM D 785
Tensile Strength, Yield 19.0 MPa
2760 psi
ASTM D 638
Elongation at Break 550 %
550 %
ASTM D 638
Flexural Modulus 0.620 GPa
89.9 ksi
Tangent, 0.05 in/min; ASTM D790
0.689 GPa
100 ksi
Tangent, 0.5 in/min; ASTM D790
Izod Impact, Notched 1.30 J/cm
2.44 ft-lb/in
73°F; ASTM D256