Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

LyondellBasell Hifaxâ„¢ ETA-3131E Thermoplastic Olefin Resin

Category Polymer , Thermoplastic
Manufacturer LyondellBasell
Trade Name Hifax™
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF LyondellBasell Hifaxâ„¢ ETA-3131E Thermoplastic Olefin Resin.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Key Features: fractional melt flow, medium modulus, extrusion grade thermoplastic olefin resin, excellent impact and stiffness balance, good practical impact, good processabilityApplications: molded-in color automotive gimp moldings, profilesDescription: Hifax ETA-3131E fractional melt flow, extrusion thermoplastic olefin resin has an excellent combination of stiffness, low temperature impact resistnace and processability. It was primarily designed for various automotive exterior moldings.Information provided by Montell Polyolefins.LyondellBasell is the successor company to Montell.
Physical Properties Metric English Comments
Density 0.910 g/cc
0.0329 lb/in³
ASTM D792
Linear Mold Shrinkage 0.011 cm/cm
0.011 in/in
Tool, Montell
Melt Flow 0.80 g/10 min

@Load 2.16 kg,
Temperature 230 °C
0.80 g/10 min

@Load 4.76 lb,
Temperature 446 °F
ASTM D1238
Mechanical Properties Metric English Comments
Hardness, Shore D 67
67
ASTM D2240
Tensile Strength, Yield 26.0 MPa
3770 psi
ASTM D638
Elongation at Break 450 %
450 %
ASTM D638
Flexural Modulus 0.830 GPa
120 ksi
Tangent at 0.05 in/min; ASTM D790A
Izod Impact, Notched 8.50 J/cm
15.9 ft-lb/in
ASTM D256A
Gardner Impact 28.0 J

@Temperature -30.0 °C
20.7 ft-lb

@Temperature -22.0 °F
ASTM D3029
Tear Strength 110 kN/m
628 pli
ASTM D624
Thermal Properties Metric English Comments
Deflection Temperature at 0.46 MPa (66 psi) 75.0 °C
167 °F
ASTM D648
Deflection Temperature at 1.8 MPa (264 psi) 48.0 °C
118 °F
ASTM D648
Copyright © lookpolymers.com All Rights Reserved