LyondellBasell Hifaxâ„¢ ETA-4161UV Thermoplastic Olefin Resin

Category Polymer , Thermoplastic
Manufacturer LyondellBasell
Trade Name Hifax™
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF LyondellBasell Hifaxâ„¢ ETA-4161UV Thermoplastic Olefin Resin.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Key Features: fractional melt flow, medium high modulus, UV-stabilized, extrusion grade thermoplastic olefin resin, excellent impact and stiffness balance, good melt strength, excellent weatherability, excellent processabilityApplications: thermoformed sheetDescription: Hifax ETA-4161UV fractional melt flow, UV-stabilized, extrusion grade thermoplastic olefin resin has an excellent combination of stiffness, impact resistane, melt strength, weatherability and processability. It was designed to accommodate specific thermoformed applications.Information provided by Montell Polyolefins.LyondellBasell is the successor company to Montell.
Physical Properties Metric English Comments
Density 0.910 g/cc
0.0329 lb/in³
ASTM D792
Melt Flow 0.50 g/10 min

@Load 2.16 kg,
Temperature 230 °C
0.50 g/10 min

@Load 4.76 lb,
Temperature 446 °F
ASTM D1238
Mechanical Properties Metric English Comments
Hardness, Shore D 70
70
ASTM D2240
Tensile Strength, Yield 28.0 MPa
4060 psi
ASTM D638
Elongation at Break 250 %
250 %
ASTM D638
Flexural Modulus 1.00 GPa
145 ksi
Tangent at 0.05 in/min; ASTM D790A
Izod Impact, Notched 7.40 J/cm
13.9 ft-lb/in
ASTM D256A
Tear Strength 110 kN/m
628 pli
ASTM D624
Thermal Properties Metric English Comments
Deflection Temperature at 0.46 MPa (66 psi) 80.0 °C
176 °F
ASTM D648
Deflection Temperature at 1.8 MPa (264 psi) 50.0 °C
122 °F
ASTM D648