LyondellBasell Lupolex FA LLDPE

Category Polymer , Film , Thermoplastic , Polyethylene (PE) , LLDPE , Linear Low Density Polyethylene (LLDPE), Film Grade
Manufacturer LyondellBasell
Trade Name Lupolex
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF LyondellBasell Lupolex FA LLDPE.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Description: Lupolex 25G FA is a linear low density polyethylene (LLDPE) used for blending, film, packaging, and bagsFeatures: AntioxidantGood Puncture ResistanceHigh RigidityHigh ClarityGood Heat SealInformation provided by Basell.
Physical Properties Metric English Comments
Density 0.925 g/cc
0.0334 lb/in³
ISO 1183
Thickness 50.8 microns
2.00 mil
Melt Flow 0.70 g/10 min

@Load 2.16 kg,
Temperature 190 °C
0.70 g/10 min

@Load 4.76 lb,
Temperature 374 °F
ISO 1133
Mechanical Properties Metric English Comments
Film Elongation at Break, MD 700 %
700 %
ISO 527
Film Elongation at Break, TD 750 %
750 %
ISO 527
Coefficient of Friction 1.1
1.1
Elenac Test Method
Dart Drop 2.36 g/micron
60.0 g/mil
ASTM D1709
Film Tensile Strength at Break, MD 35.00 MPa
5076 psi
ISO 527
Film Tensile Strength at Break, TD 35.00 MPa
5076 psi
ISO 527
Optical Properties Metric English Comments
Haze 11 %
11 %
ASTM D1003
Gloss 63 %
63 %
45°; ASTM D2457