Material Notes:
Description: Moplen Coat EP/60 Bianco fractional melt flow, 1,200 MPa flexural modulus, extrusion grade polypropylene copolymer has a very good balance of properties and processability. Available in white precolored form, this material was designed for various extrusion coating applications. Uses: coating applicationsInformation provided by Basell.
Physical Properties Metric English Comments
Density 0.902 g/cc
0.0326 lb/in³
ASTM D792
Melt Flow 0.80 g/10 min

@Load 2.16 kg,
Temperature 230 °C
0.80 g/10 min

@Load 4.76 lb,
Temperature 446 °F
Condition L; ASTM D1238
Mechanical Properties Metric English Comments
Hardness, Rockwell R 79
79
ASTM D 785
Tensile Strength at Break 25.0 MPa
3630 psi
ASTM D 638
Tensile Strength, Yield 28.0 MPa
4060 psi
ASTM D 638
Elongation at Break 500 %
500 %
ASTM D 638
Elongation at Yield 10 %
10 %
ASTM D 638
Flexural Modulus 1.10 GPa
160 ksi
Tangent, 0.05 in/min; ASTM D790
1.20 GPa
174 ksi
Tangent, 0.5 in/min; ASTM D790
Izod Impact, Notched 0.529 J/cm
0.990 ft-lb/in
(-22°F); ASTM D256
7.501 J/cm
14.05 ft-lb/in
73°F; ASTM D256