Physical Properties Metric English Comments
Specific Gravity 0.898 g/cc
0.898 g/cc
20/20°C
Density 0.899 g/cc

@Temperature 20.0 °C
0.0325 lb/in³

@Temperature 68.0 °F
Solubility in Water 100 %
100 %
20°C
Viscosity 1.8 cP

@Temperature 25.0 °C
1.8 cP

@Temperature 77.0 °F
Molecular Weight 104.1 g/mol
104.1 g/mol
Vapor Pressure 0.0133 bar

@Temperature 20.0 °C
10.0 torr

@Temperature 68.0 °F
Evaporation Loss 44 %
44 %
n-BuAc=100%
Surface Tension 29.7 dynes/cm
29.7 dynes/cm
25°C
Thermal Properties Metric English Comments
Boiling Point 132 °C
270 °F
at 760 mmHg
Flash Point 35.0 °C
95.0 °F
Seta
Optical Properties Metric English Comments
Refractive Index 1.405

@Temperature 25.0 °C
1.405

@Temperature 77.0 °F
Descriptive Properties Value Comments
CAS Number 52125-53-8
Users viewing this material also viewed the following: