LyondellBasell Petrothene® GA501020 Linear Low Density Polyethylene

Category Polymer , Film , Thermoplastic , Polyethylene (PE) , LLDPE , Linear Low Density Polyethylene (LLDPE), Film Grade
Manufacturer LyondellBasell (former Equistar)
Trade Name Petrothene®
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF LyondellBasell Petrothene® GA501020 Linear Low Density Polyethylene.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
ApplicationsPETROTHENE GA 501series of resins are pelletized linear low density polyethylene for film extrusion applications requiring excellent drawdown and toughness. These resins have excellent puncture resistance, elongation and heat seal strength. Applications include heavy duty shipping sacks, prime liners, commercial and industrial packaging, as well as food and consumer packaging. Processing TechniquesRecommended conditions are 400-450°F melt temperature and a 1.5-3.01:1 blow-up ratio. Using proper techniques, this product can readily be drawn below 0.90 mil at optimum production rates. Specific recommendations for type of resin and extrusion conditions can be made only when the end use, required properties and processing equipment are known. For further suggestions, please contact your Equistar sales representative. Regulatory StatusGA 501 series resins meet the requirements of the Food and Drug Administration regulation, 21 CFR 177.1520. This regulation allows the use of this olefin polymer in "…articles or components of articles intended for use in contact with food…" Specific limitations or conditions of use may apply. Contact your Equistar sales representative for more information. GA 501 is available without additives or fully formulated with flip and antiblock additives.Other InformationBlow-Up ratio 2.1:1.This product is from the former Equistar product line.
Physical Properties Metric English Comments
Density 0.918 g/cc
0.0332 lb/in³
ASTM D1505
Thickness 38.1 microns
1.50 mil
2:1 BUR
Melt Flow 1.0 g/10 min
1.0 g/10 min
190/2.16; ASTM D1238
Mechanical Properties Metric English Comments
Film Elongation at Break, MD 600 %
600 %
ASTM D882
Film Elongation at Break, TD 760 %
760 %
ASTM D882
Elmendorf Tear Strength MD 160 g
160 g
ASTM D1922
Elmendorf Tear Strength TD 560 g
560 g
ASTM D1922
Dart Drop Test 145 g
0.320 lb
F<sub>50</sub>; ASTM D1709A
Film Tensile Strength at Break, MD 40.0 MPa
5800 psi
ASTM D882
Film Tensile Strength at Break, TD 31.7 MPa
4600 psi
ASTM D882
1% Secant Modulus, MD 186 MPa
27000 psi
ASTM D638
1% Secant Modulus, TD 241 MPa
35000 psi
ASTM D638
Optical Properties Metric English Comments
Haze 11 %
11 %
ASTM D1003
Gloss 50 %
50 %
45°; ASTM D523
Descriptive Properties Value Comments
Antiblock None
Slip None