Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

LyondellBasell Petrothene® HR92953 Medium Density Polyethylene

Category Polymer , Thermoplastic , Polyethylene (PE) , MDPE , Medium Density Polyethylene (MDPE), Extruded
Manufacturer LyondellBasell (former Equistar)
Trade Name Petrothene®
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF LyondellBasell Petrothene® HR92953 Medium Density Polyethylene.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
ApplicationsPETROTHENE HR 92953 is a medium density polyethylene-based resin designed for use as jacketing for communications cable, including CATV and FOC. HR 92953 has a nominal carbon black content of 2.6% and antioxidant has been added to ensure thermal stability during processing.Processing TechniquesHR 92953, like other thermoplastic polyolefin compounds, can be extruded as wire and cable insulation using a conventional extruder. Below are suggested extrusion conditions for HR 92953. These conditions are intended as general guidelines only and are not optimum values, since manufacturing conditions, such as extruder type and size, affect the processing of thermoplastic compounds.This product is from the former Equistar product line.
Physical Properties Metric English Comments
Density 0.945 g/cc
0.0341 lb/in³
ASTM D1505
Environmental Stress Crack Resistance >= 1000 hour
>= 1000 hour
Condition A - 10% Igepal®; ASTM D1693
Absorption Coefficient 450
450
ASTM D3349
Carbon Black Loading 2.6 %
2.6 %
Melt Flow 0.65 g/10 min
0.65 g/10 min
ASTM D1238
Mechanical Properties Metric English Comments
Hardness, Shore D 60
60
ASTM D2240
Tensile Strength at Break 27.6 MPa
4000 psi
ASTM D638
Tensile Strength, Yield 16.5 MPa
2400 psi
ASTM D638
Elongation at Break 880 %
880 %
ASTM D638
Thermal Properties Metric English Comments
CTE, linear 175 µm/m-°C

@Temperature 20.0 °C
97.2 µin/in-°F

@Temperature 68.0 °F
ASTM D696
Brittleness Temperature <= -76.0 °C
<= -105 °F
F<sub>50</sub>; ASTM D746
Electrical Properties Metric English Comments
Dielectric Constant 2.55

@Frequency 1e+6 Hz
2.55

@Frequency 1e+6 Hz
ASTM D1531
Dielectric Strength 21.7 kV/mm
550 kV/in
DC; ASTM D149
Dissipation Factor 0.00050

@Frequency 1e+6 Hz
0.00050

@Frequency 1e+6 Hz
ASTM D1531
Processing Properties Metric English Comments
Feed Temperature 154 - 163 °C
310 - 325 °F
Zone 2 177 - 193 °C
350 - 380 °F
Zone 3 193 - 210 °C
380 - 410 °F
Zone 4-x 204 - 218 °C
400 - 425 °F
Adapter Temperature 204 - 218 °C
400 - 425 °F
Die Temperature 204 - 218 °C
400 - 425 °F