LyondellBasell Petrothene® KR92717 High Density Polyethylene

Category Polymer , Thermoplastic , Polyethylene (PE) , HDPE , High Density Polyethylene (HDPE), Extruded
Manufacturer LyondellBasell (former Equistar)
Trade Name Petrothene®
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF LyondellBasell Petrothene® KR92717 High Density Polyethylene.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
ApplicationsPETROTHENE KR 92717 is a high molecular weight, high density polyethylene-based compound designed for use in spacer cable insulation and cable jacketing applications. This black compound contains additive packages to ensure UV and processing stability.Processing TechniquesKR 92717, like other thermoplastic polyolefin compounds, can be extruded as wire and cable insulation using a conventional extruder. Below are suggested extrusion conditions for KR 92717. These conditions are intended as general guidelines only and are not optimum values, because manufacturing conditions such as extruder type and size affect the processing of thermoplastic compounds.This product is from the former Equistar product line.
Physical Properties Metric English Comments
Density 0.950 g/cc
0.0343 lb/in³
ASTM D1505
Melt Flow 0.50 g/10 min
0.50 g/10 min
ASTM D1238
Mechanical Properties Metric English Comments
Hardness, Shore D 61
61
ASTM D2240
Tensile Strength at Break 15.2 MPa
2200 psi
ASTM D638
Tensile Strength, Yield 22.1 MPa
3200 psi
ASTM D638
Elongation at Break 700 %
700 %
ASTM D638
Thermal Properties Metric English Comments
Brittleness Temperature <= -76.0 °C
<= -105 °F
F<sub>50</sub>; ASTM D746
Electrical Properties Metric English Comments
Dielectric Constant 2.3

@Frequency 1000 Hz
2.3

@Frequency 1000 Hz
ASTM D1531
2.38

@Frequency 1e+6 Hz
2.38

@Frequency 1e+6 Hz
ASTM D1531
Dissipation Factor 0.00020

@Frequency 1000 Hz
0.00020

@Frequency 1000 Hz
ASTM D1531
0.00020

@Frequency 1e+6 Hz
0.00020

@Frequency 1e+6 Hz
ASTM D1531
Processing Properties Metric English Comments
Feed Temperature 149 - 163 °C
300 - 325 °F
Zone 2 177 - 204 °C
350 - 400 °F
Zone 3 191 - 204 °C
375 - 400 °F
Zone 4-x 238 - 260 °C
460 - 500 °F
Adapter Temperature 246 - 260 °C
475 - 500 °F
Die Temperature 246 - 260 °C
475 - 500 °F
Melt Temperature 246 - 260 °C
475 - 500 °F
Copyright © lookpolymers.com All Rights Reserved