LyondellBasell Petrothene® LP5100 High Density Polyethylene

Category Polymer , Thermoplastic , Polyethylene (PE) , HDPE , High Density Polyethylene (HDPE), Blow Molding Grade
Manufacturer LyondellBasell (former Equistar)
Trade Name Petrothene®
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF LyondellBasell Petrothene® LP5100 High Density Polyethylene.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
ApplicationsPETROTHENE LP 5100 is especially designed for large-part blow molding of durable goods and deep-draw sheet extrusion/thermoforming applications. LP 5100 exhibits excellent impact resistance and ESCR.Regulatory StatusThe LP 5100 meets the requirements of Food and Drug Administration regulation, 21 CFR 177.1520. This regulation allows the use of this olefin polymer in "…articles or components of articles intended for use in contact with food." Specific limitations or conditions of use may apply. Contact your Equistar sales representative for more information. Processing TechniquesSpecific recommendations for processing LP 5100 can only be made when the processing conditions, equipment and end use are known. For further suggestions, please contact your Equistar sales representative.This product is from the former Equistar product line.
Physical Properties Metric English Comments
Density 0.950 g/cc
0.0343 lb/in³
ASTM D1505
Environmental Stress Crack Resistance >= 1000 hour
>= 1000 hour
F<sub>50</sub>; ASTM D1693
ESCR, Bottle >= 1000 hour
>= 1000 hour
F<sub>50</sub>; ASTM D2561
Melt Flow 11.5 g/10 min
11.5 g/10 min
High load; ASTM D1238
Mechanical Properties Metric English Comments
Hardness, Shore D 65
65
ASTM D2240
Tensile Strength, Yield 25.5 MPa
3700 psi
ASTM D638
Elongation at Break >= 800 %
>= 800 %
ASTM D638
Flexural Modulus 1.14 GPa
165 ksi
ASTM D790
Tensile Impact >= 107 J/cm
>= 200 ft-lb/in
ASTM D1822
Thermal Properties Metric English Comments
Deflection Temperature at 0.46 MPa (66 psi) 73.0 °C
163 °F
ASTM D648
Vicat Softening Point 122 °C
252 °F
ASTM D1525
Brittleness Temperature <= -76.0 °C
<= -105 °F
F<sub>50</sub>; ASTM D746