Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

LyondellBasell Petrothene® NA334000 Low Density Polyethylene

Category Polymer , Film , Thermoplastic , Polyethylene (PE) , LDPE , Low Density Polyethylene (LDPE), Film Grade
Manufacturer LyondellBasell (former Equistar)
Trade Name Petrothene®
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF LyondellBasell Petrothene® NA334000 Low Density Polyethylene.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
ApplicationsPETROTHENE NA 334-000 is a homopolymer resin specifically engineered for thin film applications. NA 334-000 is know for its consistency, exceptional drawdown and processability. Regulatory StatusNA 334-000 meets the requirements of the Food and Drug Administration regulation, 21 CFR 177.1520. This regulation allows the use of this olefin polymer in "…articles or components of articles intended for use in contact with food…" Specific limitations or conditions of use may apply. Contact your Equistar sales representative for more information. Processing TechniquesNA 334-000 is specifically designed to provide outstanding drawdown at maximum outputs. The melt strength properties of this resin result in excellent bubble stability. This resin can be processes over a wide range of temperatures; however, recommended conditions are melt temperatures between 300°-330°F and a blow-up ratio between 2.0-2.5:1. Using proper techniques and equipment, drawdown to 0.25 mil is feasible at commercial production rates. Specific recommendations for processing NA 334-000 can only be made when the processing conditions, equipment and end use are known. For further suggestions, contact your Equistar sales representative.Other InformationNo slip, no antiblock.Physical PropertiesThese are typical values and not to be construed as specific product limits. Data obtained from film produced in a 3.5"(89mm) blown film line, commercially available 8"(203 mm)die, 375°F(191°C) melt extrusion temperature, 2:1 BUR, 1.25 mil (32 micron)This product is from the former Equistar product line.
Physical Properties Metric English Comments
Density 0.919 g/cc
0.0332 lb/in³
ASTM D1505
Thickness 31.8 microns
1.25 mil
2.2:1 BUR
Melt Flow 6.0 g/10 min
6.0 g/10 min
ASTM D1238
Mechanical Properties Metric English Comments
Film Elongation at Break, MD 300 %
300 %
ASTM D882
Film Elongation at Break, TD 450 %
450 %
ASTM D882
Dart Drop Test 65.0 g
0.143 lb
F<sub>50</sub>; ASTM D1709
Film Tensile Strength at Break, MD 15.2 MPa
2200 psi
ASTM D882
Film Tensile Strength at Break, TD 13.8 MPa
2000 psi
ASTM D882
1% Secant Modulus, MD 138 MPa
20000 psi
ASTM D882
1% Secant Modulus, TD 159 MPa
23000 psi
ASTM D882
Optical Properties Metric English Comments
Haze 12 %
12 %
ASTM D1003
Gloss 50 %
50 %
at 45°; ASTM D2457
Processing Properties Metric English Comments
Melt Temperature 163 °C
325 °F
Copyright © lookpolymers.com All Rights Reserved