Material Notes:
Primary Processing Method: General PurposeKey Features: easy molding, FDA acceptable, general purpose polypropylene homopolymer resin, low odor transferApplications: containers, closures, hospital and institutional ware, toysMeets FDA requirements in 21 CFR 177.1520 for all food contact, including cooking applications.Description: Pro-fax 6331 general purpose polypropylene homopolymer resin is available in pellet form. This resin meets FDA requirements in the Code of Federal Regulation n 21 CFR 177.1520 for all food contact, including cooking applications. It has a UL yellow card RTI. These apply to all colors. All ingredients meet the chemical registration requirements of TSCA and DSL.Information provided by Montell Polyolefins.LyondellBasell is the successor company to Montell.
Physical Properties Metric English Comments
Density 0.900 g/cc
0.0325 lb/in³
ASTM D792B
Melt Flow 12 g/10 min

@Load 2.16 kg,
Temperature 230 °C
12 g/10 min

@Load 4.76 lb,
Temperature 446 °F
ASTM D1238
Mechanical Properties Metric English Comments
Hardness, Rockwell R 90
90
ASTM D785A
Tensile Strength, Yield 35.0 MPa
5080 psi
ASTM D638
Elongation at Yield 10 %
10 %
ASTM D638
Flexural Modulus 1.50 GPa
218 ksi
1% secant at 0.05 in/min; ASTM D790A
Izod Impact, Notched 0.350 J/cm
0.656 ft-lb/in
ASTM D256A
Thermal Properties Metric English Comments
Deflection Temperature at 0.46 MPa (66 psi) 97.0 °C
207 °F
ASTM D648
UL RTI, Mechanical with Impact 65.0 °C
149 °F
Minimum thickness 0.038 inches.
Flammability, UL94 HB
HB
Minimum thickness 0.038 inches.
Users viewing this material also viewed the following: