LyondellBasell Pro-faxâ„¢ SD183 Polypropylene Copolymer

Category Polymer , Thermoplastic , Polypropylene (PP) , Polypropylene Copolymer
Manufacturer LyondellBasell
Trade Name Pro-fax™
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF LyondellBasell Pro-faxâ„¢ SD183 Polypropylene Copolymer.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Description: Pro-fax™ SD183 medium impact polypropylene copolymer resin is extremely resistant to aging at elevated temperatures in both wet and dry environments. It has an excellent balance of properties and is suited for injection molding or extrusion applications. Pro-fax™ SD183 resin has a UL yellow card RTI of 65°C and a flame rating of UL94HB; these apply to all colors at a minimum thickness of 0.043 inches. All ingredients meet the chemical registration requirements of TSCA (U.S.) and DSL (Canada). Uses: AppliancesInformation provided by Basell.
Physical Properties Metric English Comments
Density 0.902 g/cc
0.0326 lb/in³
ASTM D792
Melt Flow 1.5 g/10 min

@Load 2.16 kg,
Temperature 230 °C
1.5 g/10 min

@Load 4.76 lb,
Temperature 446 °F
Condition L; ASTM D1238
Mechanical Properties Metric English Comments
Tensile Strength, Yield 27.6 MPa
4000 psi
ASTM D 638
Elongation at Yield 10 %
10 %
ASTM D 638
Flexural Modulus 1.17 GPa
170 ksi
1% Secant, 0.05 in/min; ASTM D790
Izod Impact, Notched 1.60 J/cm
3.00 ft-lb/in
73°F; ASTM D256
Gardner Impact 27.1 J

@Temperature -30.0 °C
20.0 ft-lb

@Temperature -22.0 °F
ASTM D3029, tested in accordance with ASTM D5420
Thermal Properties Metric English Comments
Deflection Temperature at 0.46 MPa (66 psi) 87.2 °C
189 °F
Unannealed; ASTM D648