Material Notes:
Key Features: excellent cold impact resistance, good stiffness and impact balance, UV stabilizer, polypropylene copolymer resin, injection moldingApplications: automotive interior trim, pet carriers, seatingAll ingredients meet TSCA (US) and DSL (Canada) registration requirements.Description: Pro-fax SG702 high flow, high impact polypropylene copolymer resin is designed for injection molding applications and is available in pellet form. It has a UL yellow card RTI, which applies to all colors. All ingredients meet the chemical registration requirements of TSCA and DSL.Information provided by Montell Polyolefins.LyondellBasell is the successor company to Montell.
Physical Properties Metric English Comments
Density 0.900 g/cc
0.0325 lb/in³
ASTM D792B
Melt Flow 18 g/10 min

@Load 2.16 kg,
Temperature 230 °C
18 g/10 min

@Load 4.76 lb,
Temperature 446 °F
ASTM D1238
Mechanical Properties Metric English Comments
Tensile Strength, Yield 21.0 MPa
3050 psi
ASTM D638
Elongation at Yield 5.0 %
5.0 %
ASTM D638
Flexural Modulus 1.10 GPa
160 ksi
1% secant at 0.05 in/min; ASTM D790A
Izod Impact, Notched 2.30 J/cm
4.31 ft-lb/in
ASTM D256A
Impact Test 61.0 J

@Temperature 5.00 °C
45.0 ft-lb

@Temperature 41.0 °F
Montell drop weight impact strength
Thermal Properties Metric English Comments
Deflection Temperature at 0.46 MPa (66 psi) 90.0 °C
194 °F
ASTM D648
UL RTI, Mechanical with Impact 65.0 °C
149 °F
Minimum thickness of 0.059 inches.
Flammability, UL94 HB
HB
Minimum thickness of 0.059 inches.