M. Holland Company EV200 EVA  (discontinued **)

Category Polymer , Film , Thermoplastic , Ethylene Vinyl Acetate , Ethylene Vinyl Acetate Copolymer (EVA), Film Grade
Manufacturer
Trade Name
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF M. Holland Company EV200 EVA  (discontinued **).pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Features: Good Heat Seal, Opticals, High StrengthUses: PackagingApprovals: FDA 21 CFR 177.1350 and FDA 21 CFR 176.170,Table 2, Cond. C, D, E, F, GProcessing Method: Film, BlownInformation provided by M. Holland.
Physical Properties Metric English Comments
Density 0.923 g/cc
0.0333 lb/in³
ASTM D1505
Melt Flow 2.5 g/10 min

@Load 2.16 kg,
Temperature 230 °C
2.5 g/10 min

@Load 4.76 lb,
Temperature 446 °F
ASTM D1238
Mechanical Properties Metric English Comments
Film Elongation at Break, MD 400 %
400 %
ASTM D882
Film Elongation at Break, TD 450 %
450 %
ASTM D882
Secant Modulus, MD 0.159 GPa
23.1 ksi
ASTM D882
Secant Modulus, TD 0.198 GPa
28.7 ksi
ASTM D882
Film Tensile Strength at Break, MD 22.8 MPa
3300 psi
ASTM D882
Film Tensile Strength at Break, TD 17.2 MPa
2500 psi
ASTM D882
Descriptive Properties Value Comments
Form Pellets