M. Holland Company GS230WC Polystyrene, Specialty

Category Polymer , Thermoplastic , Polystyrene (PS) , Polystyrene, Transparent Grade
Manufacturer M. Holland Company
Trade Name
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF M. Holland Company GS230WC Polystyrene, Specialty.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
High clarityCrystallineHigh heat resistanceGood mold releaseApplications: BottlesLabwareVials
Physical Properties Metric English Comments
Specific Gravity 1.05 g/cc
1.05 g/cc
23/23°C; ASTM D792
Melt Flow 3.0 g/10 min

@Load 5.00 kg,
Temperature 200 °C
3.0 g/10 min

@Load 11.0 lb,
Temperature 392 °F
ASTM D1238
Mechanical Properties Metric English Comments
Tensile Strength, Yield 53.8 MPa
7800 psi
ASTM D638
Tensile Modulus 3.17 GPa
460 ksi
ASTM D638
Flexural Modulus 3.10 GPa
450 ksi
ASTM D790
Izod Impact, Notched 0.214 J/cm
0.400 ft-lb/in
73°F; ASTM D256
Thermal Properties Metric English Comments
Vicat Softening Point 106 °C
222 °F
ASTM D1525
Descriptive Properties Value Comments
Forms Pellets
Processing Methods Injection molding