Category Polymer , Film , Thermoplastic , Polyethylene (PE) , LLDPE , Linear Low Density Polyethylene (LLDPE), Film Grade
Manufacturer
Trade Name
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF M. Holland Company MAGMA® LL1091-AS LLDPE  (discontinued **).pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Additives: Medium Antiblock, Medium SlipFeatures: Good Heat Seal, Good Processability, Good Tear Strength, Good ToughnessProcessing Method: ExtrusionInformation provided by M. Holland.
Physical Properties Metric English Comments
Density 0.919 g/cc
0.0332 lb/in³
ASTM D1505
Thickness 31.8 microns
1.25 mil
Melt Flow 1.0 g/10 min
1.0 g/10 min
ASTM D1238
Mechanical Properties Metric English Comments
Film Elongation at Break, MD 590 %
590 %
ASTM D882
Film Elongation at Break, TD 700 %
700 %
ASTM D882
Elmendorf Tear Strength MD 540 g
540 g
ASTM D1922
Elmendorf Tear Strength TD 720 g
720 g
ASTM D1922
Dart Drop Test >= 575 g
>= 1.27 lb
ASTM D1709
Film Tensile Strength at Break, MD 50.7 MPa
7350 psi
ASTM D882
Film Tensile Strength at Break, TD 41.1 MPa
5960 psi
ASTM D882
Thermal Properties Metric English Comments
Melting Point 121 °C
250 °F
Processing Properties Metric English Comments
Feed Temperature <= 149 °C
<= 300 °F
Zone 1 149 °C
300 °F
Melt Temperature 182 - 232 °C
360 - 450 °F
Die Opening 0.0810 - 0.254 cm
0.0319 - 0.100 in
Blow-up Ratio (BUR) 1.5 - 3.0
1.5 - 3.0
Descriptive Properties Value Comments
Form Pellets