M. Holland Company RP200 Polypropylene Copolymer

Category Polymer , Thermoplastic , Polypropylene (PP) , Polypropylene Copolymer
Manufacturer M. Holland Company
Trade Name
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF M. Holland Company RP200 Polypropylene Copolymer.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Features: High ClarityUses: Bottles, Food Containers Approvals: FDA 21 CFR 177.1520Processing Method: Extrusion Blow Molding, Injection Blow MoldingInformation provided by M. Holland.
Physical Properties Metric English Comments
Density 0.905 g/cc
0.0327 lb/in³
ASTM D1505
Melt Flow 2.0 g/10 min

@Load 2.16 kg,
Temperature 190 °C
2.0 g/10 min

@Load 4.76 lb,
Temperature 374 °F
ASTM D1238
Mechanical Properties Metric English Comments
Hardness, Shore D 75
75
ASTM D2240
Tensile Strength, Yield 31.0 MPa
4500 psi
ASTM D638
Flexural Modulus 1.38 GPa
200 ksi
Tangent; ASTM D790
Izod Impact, Notched 0.534 J/cm
1.00 ft-lb/in
ASTM D256
Thermal Properties Metric English Comments
Deflection Temperature at 0.46 MPa (66 psi) 97.8 °C
208 °F
Unannealed; ASTM D648
Descriptive Properties Value Comments
Form Pellets