Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

MBA Polymers ABS 4124 Recycled acrylonitrile-butadiene-styrene copolymer

Category Polymer , Renewable/Recycled Polymer , Thermoplastic , ABS Polymer
Manufacturer MBA Polymers
Trade Name
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF MBA Polymers ABS 4124 Recycled acrylonitrile-butadiene-styrene copolymer.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Available in standard black.Information provided by MBA Polymers.
Physical Properties Metric English Comments
Density 1.05 g/cc
0.0379 lb/in³
MBA Method
Melt Flow 6.0 g/10 min

@Load 3.80 kg,
Temperature 230 °C
6.0 g/10 min

@Load 8.38 lb,
Temperature 446 °F
ISO 1133
22 g/10 min

@Load 10.0 kg,
Temperature 220 °C
22 g/10 min

@Load 22.0 lb,
Temperature 428 °F
ISO 1133
Mechanical Properties Metric English Comments
Tensile Strength, Yield 40.0 MPa

@Temperature 23.0 °C
5800 psi

@Temperature 73.4 °F
ISO 527-2/50
Flexural Modulus 2.20 GPa

@Temperature 23.0 °C
319 ksi

@Temperature 73.4 °F
ISO 178
Izod Impact, Notched (ISO) 10.0 kJ/m²

@Temperature 23.0 °C
4.76 ft-lb/in²

@Temperature 73.4 °F
ISO 180/1A
Thermal Properties Metric English Comments
Deflection Temperature at 1.8 MPa (264 psi) 80.0 °C
176 °F
unannealed; ISO 75-1A
Vicat Softening Point 95.0 °C
203 °F
VST/B/50; ISO 306
104 °C
219 °F
VST/A/50; ISO 306
Processing Properties Metric English Comments
Melt Temperature 200 - 220 °C
392 - 428 °F
Extrusion Range
210 °C
410 °F
Recommended Extrusion
200 - 230 °C
392 - 446 °F
Injection Molding Range
215 °C
419 °F
Recommended Injection Molding
Mold Temperature 40.0 - 60.0 °C
104 - 140 °F
50.0 °C
122 °F
Recommended
Drying Temperature 80.0 °C

@Time 7200 - 14400 sec
176 °F

@Time 2.00 - 4.00 hour
Moisture Content <= 0.10 %
<= 0.10 %