Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

MBA Polymers PS 3122 Post-consumer recycled impact modified polystyrene

Category Polymer , Renewable/Recycled Polymer , Thermoplastic , Polystyrene (PS)
Manufacturer MBA Polymers
Trade Name
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF MBA Polymers PS 3122 Post-consumer recycled impact modified polystyrene.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Available in standard black.Information provided by MBA Polymers.
Physical Properties Metric English Comments
Density 1.04 g/cc
0.0376 lb/in³
ISO 1183
Melt Flow 6.0 g/10 min

@Load 5.00 kg,
Temperature 200 °C
6.0 g/10 min

@Load 11.0 lb,
Temperature 392 °F
ISO 1133
Mechanical Properties Metric English Comments
Tensile Strength, Yield 26.0 MPa

@Temperature 23.0 °C
3770 psi

@Temperature 73.4 °F
ISO 527-2/50
Flexural Modulus 1.90 GPa

@Temperature 23.0 °C
276 ksi

@Temperature 73.4 °F
ISO 178
Izod Impact, Notched (ISO) 8.50 kJ/m²

@Temperature 23.0 °C
4.04 ft-lb/in²

@Temperature 73.4 °F
ISO 180/1A
Processing Properties Metric English Comments
Melt Temperature 200 °C
392 °F
Recommended Injection Molding
190 - 260 °C
374 - 500 °F
Injection Molding Range
Mold Temperature 40.0 °C
104 °F
Recommended
20.0 - 80.0 °C
68.0 - 176 °F
Drying Temperature 80.0 °C

@Time 3600 - 7200 sec
176 °F

@Time 1.00 - 2.00 hour
Moisture Content <= 0.10 %
<= 0.10 %