MRC Polymers MAXTELâ„¢ 620-BK Polypropylene Copolymer

Category Polymer , Thermoplastic , Polypropylene (PP) , Polypropylene Copolymer
Manufacturer MRC Polymers
Trade Name MAXTEL™
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF MRC Polymers MAXTELâ„¢ 620-BK Polypropylene Copolymer.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
• For injection molding• Excellent process ability with high flow and high impact.Information provided by MRC Polymers Inc.
Physical Properties Metric English Comments
Specific Gravity 0.900 g/cc
0.900 g/cc
ISO 1183
Melt Flow 25 g/10 min

@Load 2.16 kg,
Temperature 230 °C
25 g/10 min

@Load 4.76 lb,
Temperature 446 °F
ISO 1133
Ash <= 1.0 %
<= 1.0 %
ISO 294
Mechanical Properties Metric English Comments
Tensile Strength 18.0 MPa
2610 psi
ISO 527
Elongation at Break 100 %
100 %
ISO 527
Flexural Strength 17.0 MPa
2470 psi
ISO 178
Flexural Modulus 0.685 GPa
99.4 ksi
ISO 178
Izod Impact, Notched (ISO) 43.0 kJ/m²
20.5 ft-lb/in²
ISO 180
Thermal Properties Metric English Comments
Deflection Temperature at 0.46 MPa (66 psi) 67.0 °C
153 °F
ISO 75
Deflection Temperature at 1.8 MPa (264 psi) 43.0 °C
109 °F
ISO 75