Material Notes:
• For extrusion or injection molding• Excellent process ability.Information provided by MRC Polymers Inc.
Physical Properties Metric English Comments
Specific Gravity 0.900 g/cc
0.900 g/cc
ISO 1183
Melt Flow 4.0 g/10 min

@Load 2.16 kg,
Temperature 230 °C
4.0 g/10 min

@Load 4.76 lb,
Temperature 446 °F
ISO 1133
Ash <= 2.0 %
<= 2.0 %
ISO 294
Mechanical Properties Metric English Comments
Tensile Strength 27.0 MPa
3920 psi
ISO 527
Elongation at Break 55 %
55 %
ISO 527
Flexural Strength 30.0 MPa
4350 psi
ISO 178
Flexural Modulus 1.15 GPa
167 ksi
ISO 178
Izod Impact, Notched (ISO) 5.30 kJ/m²
2.52 ft-lb/in²
ISO 180
Thermal Properties Metric English Comments
Deflection Temperature at 0.46 MPa (66 psi) 89.0 °C
192 °F
ISO 75
Deflection Temperature at 1.8 MPa (264 psi) 54.0 °C
129 °F
ISO 75