Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

MRC Polymers NAXELLâ„¢ PC110-20G General Purpose Polycarbonate, Medium Viscosity, 20% Glass Fiber

Category Polymer , Thermoplastic , Polycarbonate (PC) , Polycarbonate, 20% Glass Filled
Manufacturer MRC Polymers
Trade Name NAXELL™
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF MRC Polymers NAXELLâ„¢ PC110-20G General Purpose Polycarbonate, Medium Viscosity, 20% Glass Fiber.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
• Available in natural and custom colors• Can be UV Stabilized• Internal and external lubricants can be addedInformation provided by MRC Polymers Inc.
Physical Properties Metric English Comments
Specific Gravity 1.35 g/cc
1.35 g/cc
ASTM D 792
Linear Mold Shrinkage 0.0010 - 0.0030 cm/cm
0.0010 - 0.0030 in/in
ASTM D 955
Mechanical Properties Metric English Comments
Tensile Strength, Yield 103 MPa
14900 psi
ASTM D 638
Elongation at Break 5.0 %
5.0 %
ASTM D 638
Flexural Strength 131 MPa
19000 psi
ASTM D 790
Flexural Modulus 5.168 GPa
749.6 ksi
ASTM D 790
Izod Impact, Notched 1.068 J/cm

@Temperature 23.0 °C
2.001 ft-lb/in

@Temperature 73.4 °F
ASTM D 256
Thermal Properties Metric English Comments
CTE, linear 27.0 µm/m-°C
15.0 µin/in-°F
ASTM D 696
Deflection Temperature at 0.46 MPa (66 psi) 146 °C
295 °F
ASTM D 648
Deflection Temperature at 1.8 MPa (264 psi) 141 °C
286 °F
ASTM D 648