Material Notes:
• Available in natural and custom colors• Can be UV Stabilized• Internal and external lubricants can be addedInformation provided by MRC Polymers Inc.
Physical Properties Metric English Comments
Specific Gravity 1.20 g/cc
1.20 g/cc
ASTM D 792
Water Absorption 0.15 %
0.15 %
ASTM D 570
Melt Flow 4.0 g/10 min

@Load 1.20 kg,
Temperature 300 °C
4.0 g/10 min

@Load 2.65 lb,
Temperature 572 °F
ASTM D 1238
Mechanical Properties Metric English Comments
Tensile Strength, Yield 62.0 MPa
8990 psi
ASTM D 638
Elongation at Break 70 %
70 %
ASTM D 638
Flexural Strength 96.0 MPa
13900 psi
ASTM D 790
Flexural Modulus 2.343 GPa
339.8 ksi
ASTM D 790
Izod Impact, Notched 6.408 J/cm

@Temperature 23.0 °C
12.00 ft-lb/in

@Temperature 73.4 °F
ASTM D 256
Thermal Properties Metric English Comments
Deflection Temperature at 0.46 MPa (66 psi) 135 °C
275 °F
ASTM D 648
Deflection Temperature at 1.8 MPa (264 psi) 129 °C
264 °F
ASTM D 648