MV Labs AS600 AsI3 Arsenic(III) iodide

Category Ceramic , Halide
Manufacturer MV Laboratories
Trade Name
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF MV Labs AS600 AsI3 Arsenic(III) iodide.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Information provided by MV Laboratories.
Physical Properties Metric English Comments
Molecular Weight 455.64 g/mol
455.64 g/mol
Descriptive Properties Value Comments
Assay 455.64
CAS Number 7784-45-4
Form Red crystals
Purity 99.999%
Typical Impurities Sb < 5 ppm