MV Labs AU600 AuI Gold(I) iodide

Category Ceramic , Halide
Manufacturer MV Laboratories
Trade Name
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF MV Labs AU600 AuI Gold(I) iodide.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Information provided by MV Laboratories.
Physical Properties Metric English Comments
Molecular Weight 323.87 g/mol
323.87 g/mol
Descriptive Properties Value Comments
Assay 61% Au
CAS Number 10294-31-2
Form Yellow powder
Purity 99.99%
Typical Impurities Check with Manufacturer