MV Labs CD600 CdI2 Cadmium iodide

Category Ceramic , Halide
Manufacturer MV Laboratories
Trade Name
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF MV Labs CD600 CdI2 Cadmium iodide.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Information provided by MV Laboratories.
Physical Properties Metric English Comments
Molecular Weight 366.21 g/mol
366.21 g/mol
Descriptive Properties Value Comments
Assay 31% Cd
CAS Number 7790-80-9
Form White powder
Purity 99.999%
Typical Impurities Ca, Cu, Fe, Mg, Zn, Si < 1 ppm