MV Labs CU1000 CuSO4·5H2O Copper(II) sulfate pentahydrate

Category Ceramic
Manufacturer MV Laboratories
Trade Name
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF MV Labs CU1000 CuSO4·5H2O Copper(II) sulfate pentahydrate.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Information provided by MV Laboratories.
Physical Properties Metric English Comments
Molecular Weight 294.68 g/mol
294.68 g/mol
Descriptive Properties Value Comments
Assay 25% Cu
CAS Number 7758-99-8
Form Blue crystals
Purity 99.999%
Typical Impurities Fe = 3; Ag, Mg, Pb, Si < 1 ppm