MV Labs EU700 Eu(NO3)3·5H2O Europium(III) nitrate pentahydrate

Category Ceramic
Manufacturer MV Laboratories
Trade Name
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF MV Labs EU700 Eu(NO3)3·5H2O Europium(III) nitrate pentahydrate.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Information provided by MV Laboratories.
Physical Properties Metric English Comments
Molecular Weight 427.97 g/mol
427.97 g/mol
Descriptive Properties Value Comments
Assay 33% Eu
CAS Number 63026-01-7
Form White crystals
Purity 99.999%
Typical Impurities Ca, Si = 3; Ce = 2; other Rare Earths < 10 ND