MV Labs GD200 GdBr3·xH2O Gadolinium bromide hydrate

Category Ceramic , Halide
Manufacturer MV Laboratories
Trade Name
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF MV Labs GD200 GdBr3·xH2O Gadolinium bromide hydrate.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Information provided by MV Laboratories.
Physical Properties Metric English Comments
Molecular Weight 396.98 g/mol
396.98 g/mol
Descriptive Properties Value Comments
Assay 31% Gd
CAS Number 30010-20-9
Form White crystals
Purity 99.999%
Typical Impurities Check with Manufacturer