MV Labs IN500 InF3 Indium(III) fluoride

Category Ceramic , Halide
Manufacturer MV Laboratories
Trade Name
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF MV Labs IN500 InF3 Indium(III) fluoride.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Information provided by MV Laboratories.
Physical Properties Metric English Comments
Molecular Weight 171.82 g/mol
171.82 g/mol
Descriptive Properties Value Comments
Assay 67% In
CAS Number 7783-52-0
Form White powder
Purity 99.99%
Typical Impurities Check with Manufacturer