MV Labs K910 K2HPO4 Potassium hydrogen phosphate

Category Ceramic
Manufacturer MV Laboratories
Trade Name
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF MV Labs K910 K2HPO4 Potassium hydrogen phosphate.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Information provided by MV Laboratories.
Physical Properties Metric English Comments
Molecular Weight 228.22 g/mol
228.22 g/mol
Descriptive Properties Value Comments
Assay 45% K
CAS Number 7758-11-4
Form White powder
Purity 99.99%
Typical Impurities Na<50; Al, Ba, Li < 5 ppm