MV Labs NA870 Na2CO4 Sodium oxalate

Category Ceramic
Manufacturer MV Laboratories
Trade Name
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF MV Labs NA870 Na2CO4 Sodium oxalate.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Information provided by MV Laboratories.
Physical Properties Metric English Comments
Molecular Weight 134 g/mol
134 g/mol
Descriptive Properties Value Comments
Assay 34% Na
CAS Number 62-76-0
Form White powder
Purity 99.99+%
Typical Impurities K < 50; Fe, Pb < 2 ppm