MV Labs SR500 SrF2 Strontium fluoride

Category Ceramic , Halide
Manufacturer MV Laboratories
Trade Name
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF MV Labs SR500 SrF2 Strontium fluoride.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Information provided by MV Laboratories.
Physical Properties Metric English Comments
Molecular Weight 125.62 g/mol
125.62 g/mol
Descriptive Properties Value Comments
Assay 70% Sr
CAS Number 7783-48-4
Form White powder
Purity 99.99%
Typical Impurities Si = 35; Ba, Ca = 10 ppm