Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

MV Labs ZN200 ZnBr2 Zinc bromide

Category Ceramic , Halide
Manufacturer MV Laboratories
Trade Name
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF MV Labs ZN200 ZnBr2 Zinc bromide.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Information provided by MV Laboratories.
Physical Properties Metric English Comments
Molecular Weight 225.19 g/mol
225.19 g/mol
Descriptive Properties Value Comments
Assay 29% Zn
CAS Number 7699-45-8
Form White powder
Purity 99.999%
Typical Impurities Ca, Cd = 4; Fe, Mg, Mn < 1 ppm
Users viewing this material also viewed the following: