Information provided by MV Laboratories.
Physical Properties Metric English Comments
Molecular Weight 103.37 g/mol
103.37 g/mol
Descriptive Properties Value Comments
Assay 63% Zn
CAS Number 7783-49-5
Form White powder
Purity 99.99%
Typical Impurities Si < 10; Cd = 3; Ca, Fe, Mg, Mn < 1 ppm