Magyar Aluminum ALO-G22-10 Alumina

Category Ceramic , Oxide , Aluminum Oxide
Manufacturer Magyar Aluminium
Trade Name
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Magyar Aluminum ALO-G22-10 Alumina.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Ground Alumina
Physical Properties Metric English Comments
Particle Size 7.0 - 13 µm
7.0 - 13 µm
d50
45 µm
45 µm
1% max, wet sieve
Specific Surface Area 140 - 190 m²/g
140 - 190 m²/g
BET
Component Elements Properties Metric English Comments
Al2O3 >= 91 %
>= 91 %
Determined by difference
Fe2O3 <= 0.040 %
<= 0.040 %
Loss on Ignition(%) <= 8.0 %
<= 8.0 %
Na2O <= 0.40 %
<= 0.40 %
SiO2 <= 0.040 %
<= 0.040 %