Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Mallard Creek Polymers BarrierPro® 4550 SBR Emulsion

Category Polymer , Thermoset , Rubber or Thermoset Elastomer (TSE) , Styrene Butadiene Rubber
Manufacturer Mallard Creek Polymers
Trade Name BarrierPro®
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Mallard Creek Polymers BarrierPro® 4550 SBR Emulsion.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
BARRIER PRO® 4550 is an anionic carboxylated styrene-butadiene copolymer latex containing a non-staining antioxidant. Features: highly stable, good compatibility with fillers and pigments, etc., cured films are tough and flexible, cured films have good water resistance, hydrolysis resistant. STORAGE AND HANDLING: Protect from freezing. Ideal storage temperature is 22°C (72°F). Stability at 22°C (72°F) is 180 days when properly stored. Read the BARRIER PRO® 4550 Material Safety Data Sheet before handling, storing, or using this product.APPLICATIONS: BARRIER PRO ® 4550 is a general purpose latex binder of medium stiffness. It dries to form a flexible, tough film of high water resistance. BARRIER PRO® 4550 can be compounded with fillers and other additives to form coatings for a variety of applications such as damp proof membranes, specialty paints and sealants.Information provided by Mallard Creek Polymers
Physical Properties Metric English Comments
Solids Content 49 - 51 %
49 - 51 %
pH 9.5 - 10
9.5 - 10
Brookfield Viscosity <= 900 cP
<= 900 cP
#2/20 rpm
Thermal Properties Metric English Comments
Glass Transition Temp, Tg 1.00 °C
33.8 °F
Users viewing this material also viewed the following: