Mallard Creek Polymers ROVENE® 4180 SBR Latex

Category Polymer , Thermoset , Rubber or Thermoset Elastomer (TSE) , Styrene Butadiene Rubber
Manufacturer Mallard Creek Polymers
Trade Name
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Mallard Creek Polymers ROVENE® 4180 SBR Latex.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
ROVENE® 4180 is a carboxylated styrene-butadiene emulsion that has a firm hand with excellent strength properties. This binder is a low VOC containing latex that is cross-linkable with external cross-linking agents. ROVENE® 4180 can be compounded to high solids using calcium carbonate, clays, and alumina trihydrate as fillers; sodium polyacrylate thickeners are commonly used to obtain the required application viscosity. ROVENE® 4180 imparts good wet/dry tensile strength, and has good adhesion to a wide variety of surfaces. This product is recommended for a wide variety of applications, including those that require water resistance.APPLICATIONS: ROVENE® 4180 is recommended for use in industrial coatings, paper saturation/coatings, laminations, water resistant coatings, and specialty nonwoven/textile applications.Information provided by Mallard Creek Polymers
Physical Properties Metric English Comments
Solids Content 54.5 - 55.5 %
54.5 - 55.5 %
Particle Size 0.18 µm
0.18 µm
pH 7.0 - 7.5
7.0 - 7.5
Brookfield Viscosity 200 - 1500 cP
200 - 1500 cP
#2/20 rpm
Thermal Properties Metric English Comments
Glass Transition Temp, Tg 12.0 °C
53.6 °F
Chemical Properties Metric English Comments
Styrene Content 62 %
62 %
Descriptive Properties Value Comments
Emulsifiers Anionic