Mallard Creek Polymers ROVENE® 5010 SBR Latex

Category Polymer , Thermoset , Rubber or Thermoset Elastomer (TSE) , Styrene Butadiene Rubber
Manufacturer Mallard Creek Polymers
Trade Name
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Mallard Creek Polymers ROVENE® 5010 SBR Latex.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
ROVENE® 5010 is a carboxylated styrene-butadiene emulsion that imparts an ultra soft hand when used in backcoating, spray, and “dip and nip” applications. This non-woven, textile, and paper binder offers excellent water and solvent resistance when formulated with external crosslinking resins. It gives good adhesion to polyester as well as cellulosic substrates, and was designed to have excellent pad roll stability.APPLICATIONS: ROVENE® 5010 is recommended for non-woven and textile applications that require an ultra soft and strong backcoating. Its ability to be crosslinked with external crosslinkers has extended its uses in textile and non-wovens where high solvent and water resistance is required. ROVENE® 5010 has also found extensive use in paper saturation for paper tape applications.Information provided by Mallard Creek Polymers
Physical Properties Metric English Comments
Solids Content 52 - 54 %
52 - 54 %
Particle Size 0.19 µm
0.19 µm
pH 8.5 - 9.0
8.5 - 9.0
Brookfield Viscosity 175 - 800 cP
175 - 800 cP
#2/20 rpm
Thermal Properties Metric English Comments
Glass Transition Temp, Tg -26.0 °C
-14.8 °F
Chemical Properties Metric English Comments
Styrene Content 45 %
45 %
Descriptive Properties Value Comments
Emulsifiers Anionic