Mallard Creek Polymers ROVENE® 5550 SBR Latex

Category Polymer , Thermoset , Rubber or Thermoset Elastomer (TSE) , Styrene Butadiene Rubber
Manufacturer Mallard Creek Polymers
Trade Name
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Mallard Creek Polymers ROVENE® 5550 SBR Latex.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
ROVENE® 5550 is a carboxylated styrene-butadiene emulsion that has a soft, resilient hand with outstanding strength properties. This Self-crosslinking binder imparts excellent water and solvent resistance, excellent tensile strength, and good adhesion to a wide variety of fibers. In contrast to conventional SBR polymers, ROVENE® 5550 has much faster cure rated. In addition, it can be sprayed easily, is mechanically stable (at pH 8.5 or higher), and is low foaming.APPLICATIONS: ROVENE® 5550 is recommended for nonwoven and textile applications that require a self-crosslinking latex. In areas like wet wipes, polishing pads, filters, and facial scrub pads.Information provided by Mallard Creek Polymers
Physical Properties Metric English Comments
Solids Content 49 - 51 %
49 - 51 %
Particle Size 0.17 µm
0.17 µm
pH 8.7 - 9.2
8.7 - 9.2
Brookfield Viscosity 200 - 1000 cP
200 - 1000 cP
#2/20 rpm
Thermal Properties Metric English Comments
Glass Transition Temp, Tg -25.0 °C
-13.0 °F
Chemical Properties Metric English Comments
Styrene Content 45 %
45 %
Descriptive Properties Value Comments
Emulsifiers Anionic
Copyright © lookpolymers.com All Rights Reserved